Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the wordpress-seo domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /var/www/html/wp-includes/functions.php on line 6260 Shielding Velour Sunscreen Developed by Siltech - Happi
Skin Care, Sun Care

Shielding Velour Sunscreen Developed by Siltech

Formula contains Silube PCH, Silwax D02, Silmer Q25 and Silwax J1032.

Released By Siltech Corporation

Shielding Velour Sunscreen Developed by Siltech
Ingredients
%

Phase A

  • D.I. Water
  • 30.00
  • Glycerin
  • 5.00
  • Sodium chloride
  • 1.00

Phase B-1

  • Silube PCH (Siltech) (Polyglyceryl-4, Isostearate, Cetyl PEG/PPG-10/1 Dimethicone, Hexyl Laurate)
  • 6.50
  • Silwax D02 (Siltech) (Ethyl Methicone)
  • 1.00
  • Silmer Q25 (Siltech) (Trimethylsiloxysilicate)
  • 3.00
  • Silwax J1032 (Siltech) (C32 Alkyl Dimethicone)
  • 2.00
  • Silmer G-162-F5 (Siltech) (Dimethicone, Dimethicone/Vinyl Dimethicone Crosspolymer)
  • 4.00
  • Magnesium Stearate
  • 1.00
  • Siltech AP7-061 EXP (Siltech) (Triethoxyoctylsilane)
  • 5.00

Phase B-2

  • Siltech CE-2000 (Siltech) (Trioctyldodecyl Citrate)
  • 5.00
  • Tinasorb S (BASF) (Bis-ethylehexyloxyphenol Methoxyphenyl Triazine)
  • 5.00
  • Neo Heliopan 357 (Symrise) (Butyl Methoxydibenzoylmethane)
  • 3.00
  • Neo Heliopan AV (Symrise) (Trioctyldodecyl Citrate)
  • 7.50
  • ZinClear IM 50CCT (Antaria) (Zinc Oxide (and) Coco-Caprylate/Caprate (and) Polyglyceryl-3 Polyricinoleate (and) Isostearic Acid)
  • 13.50

Phase C

  • DIM2F650T4 (Kobo) (TiO2, Dimethicone, Polyglyceryl-3, Polydimethylsiloxyethyl Dimethicone, Amunia, Hydrogen Dimethicone)
  • 7.50

Phase D

  • Symocide (Symrise) (Phenoxyethanol, Decylene Glycol, 1,2-Hexanediol)
  • q.s.

Procedure

Combine liquids in Phase B1 and disperse Magnesium Stearate until homogenous. Add elastomer, mix well, then heat to 85°C. Combine Phase B2 (except ZnO); heat up to 85°C slowly under moderate mixing rate. Homogenize batch until it is uniform and then cool to room temperature. Combine ingredients in Phase A, mix well. Add Phase A to Phase B slowly under moderate mixing. Add Phase C and Phase D, one by one, under moderate mixing rate.

More Information

Siltech 416-424-4567 www.siltech.com

Request more information from Siltech Corporation